Home > News > Content

Operating Procedure Of Carburizing Furnace

- Jul 18, 2017 -

1. Close the power switch.

2, adjust the instrument (such as the right figure) after the automatic control device to allow ohmic heating.

3. When heating up, activate the fan.

4. When the furnace temperature rises to 850 ℃, it begins to drip into kerosene (or methanol).

5. After the temperature is needed, the power of the furnace and the fan can be cut off to fit the workpiece. Then fasten the door, connect the fan and stove power, operate by scope.


Related News

Related Products

  • Controlled Atmosphere Copper Continuous Bright Annealing Heat Treatment Electrical Resistance Furnace
  • Gas Carburizing Atmosphere Quenching and Tempering Heat Treatment Furnace
  • Large Capacity Bogie Hearth Type Annealing Furnace Manufactures
  • Controlled Atmosphere Bright Solution Annealing Heating Furnace
  • Practical Pit Type Electric Quenching and Tempering Furnace Used for Brake Disc and Cutter
  • Batch Pit Type Gas Carburizing Heat Treatment Furnace for Carbon Steel Parts